WC-10Co4Cr Carbides bubuk kanggo mesin umum
Katrangan
KF-65 minangka bubuk WC-10Co4Cr kualitas premium sing wis dirancang kanggo nyukupi kabutuhan industri petroleum, kertas, lan mesin umum.Produk iki nduweni kisaran ukuran partikel serbaguna 15-45 / 10-38 / 5-30 / 5-15 / 5-25μm, saéngga cocog kanggo macem-macem aplikasi.
KF-65 kasedhiya ing rong wujud: sinter & crush, lan agglomerated & sintered.Wangun sinter & crush digawe kanthi sintering bubuk banjur diremuk dadi partikel sing luwih cilik, dene wangun agglomerated & sintered digawe kanthi nglumpukake bubuk dadi partikel sing luwih gedhe sadurunge sintering.Versatility iki ndadekake gampang kanggo nggabungake KF-65 menyang proses manufaktur lan entuk asil sing dikarepake.
Salajengipun, KF-65 sebanding karo produk unggulan liyane kayata AMPERIT 554/556/557/558, METCO/AMDRY 5843/5163, WOKA 3903/3615/3652/3655/3665, PRAXAIR WC-113/1 / WC-7311350, lan PAC 1500. Iki mesthekake yen sampeyan nampa produk saka kualitas dhuwur sing ketemu standar padha merek industri-leading liyane.
Salah sawijining keuntungan utama KF-65 yaiku kemampuan kanggo dadi alternatif kanggo plating kromium keras.Iki minangka pertimbangan penting kanggo perusahaan sing pengin nyuda dampak lingkungan lan tundhuk karo peraturan.Kajaba iku, KF-65 bisa nyedhiyakake permukaan sing luwih alus, nyuda utawa malah ngilangi kabutuhan pasca mesin.Iki bisa ngirit wektu lan dhuwit ing proses manufaktur, nalika isih ngasilake asil sing bermutu.
Apa sampeyan pengin nambah kinerja peralatan, nyuda dampak lingkungan, utawa mung nambah kualitas produk, KF-65 minangka pilihan sing apik.Iki minangka solusi sing dipercaya lan larang regane sing bisa nyukupi panjaluk saka macem-macem industri, kalebu minyak bumi, kertas, lan mesin umum.Coba dina iki lan nemu bedane dhewe.
Produk sing padha
Merk | Jeneng produk | AMPERIT | METCO/AMDRY | WOKA | PRAXAIR | PAC |
KF-65 | WC-10Co4Cr | 554 | 5843 | 3903 | WC-113WC-436-1 | |
WC-10Co4Cr | 556 / 557 / 558 | 5163 | 3651 / 36523655 / 3665 | WC-7311350 | 1500 | |
WC-10Co4Cr | . | . | 3660FC | . | 1500 |
Spesifikasi
Merk | Jeneng produk | Ukuran partikel (μm) | Kimia (wt%) | Jinis | Kapadhetan katon | Flowability | Properti | Aplikasi | |||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Co | C | Fe | W | Cr | B | Si | Ni | ||||||||
KF-65 | WC-10Co4Cr | 15-45, 10-38 | 9.5-10 | 5.3-5.6 | ≤0.8 | Bal. | 3.5-4.0 | Sinter&Crush | 5.5-6.5g/cm3 | ≤25 s/50g | APS, HVOF, HVAF | Alternatif hard chromium plating;Petroleum, kertas, mesin umum | |||
KF-65 | WC-10Co4Cr | 15-45,10-38,5-30 | 9.5-10 | 5.3-5.6 | ≤0.8 | Bal. | 3.5-4.0 | Agglomerated lan sintered | 4,0-6,0 g/cm3 | ≤18 s/50g | APS, HVOF, HVAF | Alternatif hard chromium plating;Petroleum, kertas, mesin umum | |||
KF-65 | WC-10Co4Cr | 5-25,5-15 | 9.5-10 | 5.3-5.6 | ≤0.8 | Bal. | 3.5-4.0 | Agglomerated lan sintered | 3,5-4,8 g/cm3 | Pakan stabil kanggo feeder bubuk | HVOF, HVAF | Alternatif hard chromium plating; lumahing Gamelan, kurang utawa free kirim mesin; | |||
KF-60 | WC-12 Kab | 15-45, 10-63 | 10.5-12 | 4.9-5.4 | ≤0.8 | Bal. | Sinter&Crush | 5,5-6,5 g / cm3 | ≤25 s/50g | APS, HVOF | Wear resistance,Resistensi nyandhang fretting | ||||
KF-60 | WC-12 Kab | 15-45, 10-38, 5-30 | 10.5-12 | 4.9-5.4 | ≤0.8 | Bal. | Agglomerated lan sintered | 4,0-6,0 g/cm3 | ≤18 s/50g | APS, HVOF, HVAF | Wear resistance,Fretting wear resistance;mesin umum | ||||
KF-61 | WC-17 Kab | 15-45, 10-38 | 15.5-17 | 4.5-5.1 | ≤0.8 | Bal. | Agglomerated lan sintered | 3,5-5,5 g / cm3 | ≤25 s/50g | APS, HVOF, HVAF | Nyandhang resistance, fretting nyandhang resistance, kateguhan luwih apik; mesin umum | ||||
KF-62 | WC-25Co | 15-45, 10-38 | 22-26 | 4.0-4.6 | ≤0.8 | Bal. | Agglomerated lan sintered, Densification | 3,0-5,5 g/cm3 | ≤25 s/50g | APS, Detonasi bedhil, semprotan kadhemen | Fretting wear resistance,Kateguhan sing luwih apik | ||||
KF-66 | WC-23%CrC-7Ni | 15-45, 10-38 | 6.0-6.8 | ≤0.8 | Bal. | 16.5-20 | 5.5-7 | Agglomerated lan sintered | 3.0-5.0 g/cm3 | ≤25 s/50g | APS, HVOF, HVAF | Alternatif hard chromium plating; Digunakake kanggo asam konsentrasi kurang / lingkungan alkalin ing 200 ℃;Anti oksidasi lan nyandhang resistance ing 750 ℃ | |||
KF-66 | 43WC-43%CrC-14Ni | 15-45,10-38 | 7.8-8.4 | ≤0.8 | Bal. | 35-38 | 12-14 | Agglomerated lan sintered | 2.0-4.0 g/cm3 | ≤35 s/50g | APS, HVOF, HVAF | Alternatif hard chromium plating Digunakna kanggo konsentrasi asam/alkali lingkungan kurang ing 200 ℃ | |||
KF-63 | WC-10Ni | 15-45,10-38 | 4.5-5.2 | ≤0.1 | Bal. | 8.5-10.5 | Agglomerated lan sintered | 4,0-6,0 g/cm3 | ≤18 s/50g | APS, HVF, HVAF | Lapisan non-magnetik tahan aus.Resistance korosi sing luwih apik | ||||
KF-70 | Cr3C2-25NiCr | 15-45, 20-53 | 9-11 | ≤1 | Bal. | 18-21.5 | Agglomerated lan sintered | ≥2,3 g/cm3 | Pakan stabil kanggo feeder bubuk | APS, HVOF | Anti oksidasi lan nyandhang resistance ing 815 ℃ | ||||
KF-69 | Cr3C2-20NiCr | 15-45, 20-53 | 9-11 | ≤1 | Bal. | 15-17.5 | Agglomerated lan sintered | ≥2,3 g/cm3 | Pakan stabil kanggo feeder bubuk | APS, HVOF | Anti oksidasi lan nyandhang resistance ing 815 ℃ | ||||
KF-71 | Cr3C2-30NiCr | 15-45, 20-53 | 9-11 | ≤1 | Bal. | 15-17.5 | Agglomerated lan sintered | ≥2,3 g/cm3 | Pakan stabil kanggo feeder bubuk | APS, HVOF | Anti oksidasi lan nyandhang resistance ing 815 ℃.Kateguhan sing luwih apik | ||||
KF-60 | WC-12Co (Karbon Kurang) | 15-45, 20-53 | 10.5-12 | 4.0-4.4 | ≤0.8 | Bal. | Agglomerated lan sintered | 4,0-6,0 g/cm3 | ≤18 s/50g | HVOF, HVAF | Digunakake kanggo Zn bath nggulung ing Terus Galvanizing Lines | ||||
KF-68 | WC-30WB-10Co | 15-45,20-53,10-38 | 9-11 | 3.5-3.9 | Bal. | 1.4-1.7 | Agglomerated lan sintered | 3,0-4,9 g/cm3 | ≤30 s/50g | HVOF, HVAF | Digunakake kanggo Zn bath nggulung ing Terus Galvanizing Lines | ||||
KF-68 | WC-30WB-5Co5Cr | 15-45,20-53,10-38 | 4-6 | 3.5-3.9 | Bal. | 4-6 | 1.4-1.7 | Agglomerated lan sintered | 3,0-4,9 g/cm3 | ≤30 s/50g | HVOF, HVAF | Digunakake kanggo Zn bath nggulung ing Terus Galvanizing Lines | |||
KF-300E | 35% WC-NiCrBSi | 15-53,45-104 | 2.5-3.2 | 1.0-2.6 | 32-35 | 7.5-9 | 1.5-1.9 | 2.0-2.7 | Bal. | WC lan NiCrBSi mbentuk alloy | 4,0-4,9 g/cm3 | ≤16 s/50g | HVOF, PS | Tipe Campuran Alternatif WC + Ni60 ; Pemanfaatan materi sing luwih dhuwur , Konsumsi energi sing luwih murah, impact termal sing luwih murah ; Digunakake kanggo cetakan kaca | |
KF-300F | 50% WC-NiCrBSi | 15-53,45-104 | 3.2-4.3 | 0.8-2.0 | 45-48 | 5.8-7.2 | 1.0-1.7 | 1.5-2.4 | Bal. | WC lan NiCrBSi mbentuk alloy | 5,0-7 g/cm3 | ≤16 s/50g | HVOF, PS | Tipe Campuran Alternatif WC + Ni60 ; Pemanfaatan materi sing luwih dhuwur , Konsumsi energi sing luwih murah, impact termal sing luwih murah ; Digunakake kanggo cetakan kaca |